Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.74 g/cc | 0.0990 lb/in³ | |
Mykroy/Mycalex MM 800 Machining Grade Glass-bonded Mica Composite MM 800 (formerly MM 1600) is a compression molded glass mica composite that is the perfect alternative to high performance plastics where high temperature, good dielectric strength and good arc resi.. |
|||
Density | 2.74 g/cc | 0.0990 lb/in³ | |
Pyrotek Pyrocast ZC Refractory Shapes Aggregate Base: MulliteApplicationsDoor sill Breech plug Door jamb Information provided by Pyrotek. |
|||
Density | 2.74 g/cc | 0.0990 lb/in³ | |
Ferro EG 2738 Dental Glass Glass Type: Ba-Al-B-Si Typical Application: Glass Filler Ferro's Dental Glasses are standard x-ray opaque glass powders and inorganic fillers for use in dental restorations. Ferro also manufacture.. |
|||
Density | 2.74 g/cc | 0.0991 lb/in³ | |
Imerys 160D Ground Mica 160D is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution.Information provided by Imerys |
|||
Density | 2.74 g/cc | 0.0991 lb/in³ | |
Imerys 325D Ground Mica 325D Mica is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution.Information provided by Imerys |
|||
Density | 2.74 g/cc | 0.0991 lb/in³ | |
Imerys 325FFâ„¢ Ground Mica Information provided by Imerys |
|||
Density | 2.74 g/cc | 0.0991 lb/in³ | |
Imerys AMCâ„¢ 150 Ground Mica AMC 150 is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution. The inherent platy nature of AMC 150 enhances the release performance (anti-tack) in .. |
|||
Density | 2.74 g/cc | 0.0991 lb/in³ | |
Imerys AMCâ„¢ 50 Ground Mica AMC 50 Mica is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution.Information provided by Imerys |
|||
Density | 2.74 g/cc | 0.0991 lb/in³ | |
Imerys AMCâ„¢ Ground Mica AMC Mica is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution. The platy nature of AMC Mica contributes to improved crack resistance in formulted, .. |
|||
Density | 2.74 g/cc | 0.0990 lb/in³ | |
Schott S8008G Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
Density | 2.74 g/cc | 0.0990 lb/in³ | |
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus.. |