Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.65 g/cc | 0.0957 lb/in³ | |
Ferro CS 713 Metal Sealing Glass Type: Si-Ba Alkali Typical Powder Form: VSD Typical Application: Compress.Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched se.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | Apparent |
Gouda Vuurvast AK 70 K Dense Refractory Brick Description: A high quality andalusite/corundum brick with a mullite bond with a very good volume stability. Also good slag- and thermal shock resistance.Remarks: This data represents average values.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | Apparent |
Gouda Vuurvast AK 80 Dense Refractory Brick Description: A bauxite based quality with a high abrasion resistance. Widely used in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standa.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | Apparent |
Gouda Vuurvast LP 60 A Dense Refractory Brick Description: This quality combines a dense structure with a very good thermal shock resistance. The extremely low porosity results in a very good slag resistance, a good abrasion resistance and high.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | Apparent |
Gouda Vuurvast LP 60 AAP Dense Refractory Brick Description: Special low porosity quality for use under severe corrosive conditions, (for instance liquid slags). Moreover, this brick has been extra protected against slag attack because it also co.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | Apparent |
Gouda Vuurvast AK 70 A Dense Refractory Brick Description: This brick is made of a high quality bauxite. Application: transition zone of rotary cement kiln.Remarks: This data represents average values, obtained from samples that were cut from s.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | Apparent |
Gouda Vuurvast AK 70 KP Dense Refractory Brick Description: A high quality phosphate bonded andalusite/corundum brick with very good volume stability. Also good slag resistance and thermal shock resistance. Remarks: This data represents average .. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | |
Schott N-F2 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | |
Goodfellow Alumino-silicate Glass Ceramic SiO2 57/Al2O3 36/CaO/MgO/BaOPorous ceramics can be used as filters and for the controlled release of volatile chemicals. In this material, Alumino-Silicate particles are found in a glassy matrix. Th.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | ASTM-C 20 |
CoorsTek Boron Carbide Reaction-Bonded Boron Carbide Lowest density for ultra-lightweight designs |
|||
Density | 2.65 - 2.70 g/cc | 0.0957 - 0.0975 lb/in³ | |
Aremco Ceramabond™ 885 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Density | 2.65 g/cc | 0.0957 lb/in³ | |
Aleris AA5024-H116 Aluminum Magnesium Scandium Alloy Features good weldability, excellent damage tolerance, good corrosion resistance, creep-formability. Aleris AlMgSc alloy AA5024 H116 allows simplification of the manufacturing process of aircraft f.. |