Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.54 g/cc | 0.0916 lb/in³ | |
Hardwire 12x-23-12 High Density Tape The 12X Hardwire is a high carbon steel cord with a micro-fine brass or AO-brass (Adhesion Optimized) coating. The 12X wire cord is used where the traits of high tensile strain, excellent conformabi.. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | |
Schott Nextrema® 724-3 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | |
Schott Nextrema® 724-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0254 C 75% Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium Sulfate, 75% Filler by WeightFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0254 S Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | ASTM D792 |
Techmer ES HiFill® PP 0254 S1 003 Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: Good Corrosion ResistanceInformation provided by TP Composites, Inc. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0254 B Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific GravityInformation provided by TP Composites, Inc. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 0254 B2 Barium Sulfate Filler Availability: North AmericaForms: PelletsFiller/Reinforcement: Barium SulfateFeatures: High Specific Gravity and AntistaticAdditive: AntistaticInformation provided by TP Composites, Inc. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | |
Zircar Ceramics Z-MAG-B Non-RCF Blanket Mechanically needled silica magnesia fiber blanket provides much of the same performance found in ceramic fiber blanket but in a NON RCF composition.Information provided by Zircar Ceramics. |
|||
Density | 2.54 g/cc | 0.0918 lb/in³ | Fibre |
Hexcel® HexPly® M56 180°C (350°F) Out-of-Autoclave Curing Matrix, M56/37%/7581 Fiber: E-Glass, Weave: 8HS, 300 g/m2Information provided by HexCel |