Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Ferro EG 2782 Specialty Glass Glass Type: Ca-Si-B Typical Powder Form: VWG Typical Application: Sintering Aid Ferro offers a wide range of compositions for specialty applications including sintering aids used in the glass-phase.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | 2.52 g/cc Average. Minimum bulk density is 2.513 g/cc. |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Schott KG3 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG2, KG1, KG4, KG5 |
|||
Density | 2.52 g/cc @Temperature 25.0 °C |
0.0910 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8625 Biocompatible Glass Biocompatible glass, high IR-absorbing, Transponders (implantable) The heavy metal content of the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by S.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Schott K10 Glass Information Provided by SCHOTT North America, Inc. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Schott Nextrema® 712-8 Glass Ceramic The NEXTREMA® family of glass-ceramics combines the glossy appearance of glass with exceptional thermal, chemical, optical and mechanical properties such as:Very low coefficient of linear thermal.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | Typical value, After dried @ 110°C/24 hrs |
Sharadaa Ceramics REFPLAST 60 60% Alumina Plastic Nature of bond: Chemical-CeramicInstallation: Pneumatic rammingInformation provided by Sharadaa Ceramics Pvt. Ltd. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Schott KG2 Short Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include KG1, KG3, KG4, KG5 |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Corning Macor® Machinable Glass Ceramic The CTE of Macor® matches most metals and sealing glasses. It is nonwetting, exhibits zero porosity, and, unlike ductile materials, will not deform. It is an excellent insulator at high voltages,.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Accuratus MACOR Machinable Glass Ceramic Macor is cast as a two phase glass. After casting, it is heat treated causing crystallization of one phase giving rise to its glass-like and ceramic-like characteristics.Key Properties of MACOR: Mac.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Astro Met Macor® Machinable Glass Ceramic General Description:Macor is a machinable glass-ceramic material with a unique combination of useful properties. A product of Corning Incorporated, it is stocked, distributed and fabricated by Astro.. |
|||
Density | 2.52 g/cc | 0.0910 lb/in³ | |
Aremco AREMCOLOX™ 502-800 Macor® Machinable Glass Ceramic, MGC Recommended for temperatures to 1472°F (800°C) and peaks up to 1832°F (1000°C). Demonstrates low thermal conductivity, high strength, high electrical insulation, zero porosity, non-wetting, and .. |