Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 2.19 g/cc @Temperature 25.0 °C |
0.0791 lb/in³ @Temperature 77.0 °F |
|
Schott Glass 8230 Intermediate sealing glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 100 ppmInformation provided by SCHOTT AG. |
|||
Density | 2.19 g/cc | 0.0791 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 2.19 g/cc | 0.0791 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp RX06324 PA 66 (Asia Pacific) This material is Mineral filled Nylon grade with high dielectric constantThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 2.19 - 2.49 g/cc | 0.0791 - 0.0900 lb/in³ | Green |
CeramTec Ceramtape A Alumina for Constrained Sintering LTCC (Low Temperature Cofired Ceramic) is a new type of ceramic film developed by CeramTec AG's Electronics division. With the aid of these ceramics and their almost shrinkage-free sintering process.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 006 75% Virgin PTFE, 25% Glass Fiber Applications & Industries:General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperatures.. |
|||
Density | 2.19 - 2.27 g/cc | 0.0791 - 0.0820 lb/in³ | BS2782:Pt6 |
Dalau Dalcon 025 75% Virgin PTFE, 25% Glass Fiber, Blue Applications & Industries: General: 25% Glass fibre is the most widely used filler. It improves the creep resistance, compressive strength, rigidity, and wear of PTFE, both at low & high temperature.. |
|||
Density | 2.19 g/cc | 0.0791 lb/in³ | ASTM D792 |
Saint-Gobain Fluoroloy® A30 High Performance PTFE/Glass Seal Material Excellent heat, wear, and chemical resistance; Good cryogenic properties; Can be abrasive running against soft metals at high surface speed; Excellent material for back-up rings
Information .. |
|||
Density | 2.19 - 2.22 g/cc | 0.0791 - 0.0802 lb/in³ | molded; ASTM D792 |
Guarniflon PTFE G403 Polytetrafluoroethylene 15% Glass Fiber PTFE G Standard Compound with glass fiberProperties: Enhanced wear resistance. Enhanced chemical resistance (except for alkali and hydrofluoric acid).Applications: Valve seats, seals, bearings, re.. |