Physical Properties Metric English Comments
Density 2.04 g/cc
0.0737 lb/in³
Plastcom SLOVALEN PH 61 B 70 PP, 70% mineral filling
FeaturesModified PP for injection moulding with the content of 70% of barium sulphate. Increased density. Decreased shrinkage.Used for production of vertical blind weights. Delivered in natural mode..
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Europe-Africa-Middle East)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66
LNP* KONDUIT* RTF2B is a compound based on Nylon 66 resin containing 10% Glass Fiber, 55% Thermal Filler. Added features of this material include: Thermally Conductive.
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
SABIC Innovative Plastics LNP KONDUIT RTF2B PA 66 (Asia Pacific)
LNP* Konduit* RTF2B is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Thermal Filler. Added features of this material include: Thermally Conductive.
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
3M Dyneon™ CC191-HE PTFE, 25% Carbon/Graphite Filled  (discontinued **)
Product Form: Black, non-pelletized powder. Applications include bearings, bushings.Data provided by Dyneon.
Density 2.04 g/cc
0.0737 lb/in³
Meilian Chemical PE12055 WHITE MASTERBATCH
WHITE PE12055 is an economy white low density polyethylene based masterbatch containing premium TiO2 and calcium carbonate filler without any content of fluorescence whitener. This product is design..
Density 2.04 - 2.10 g/cc
0.0737 - 0.0759 lb/in³
extruded; ASTM D792
Guarniflon PTFE G453 Polytetrafluoroethylene 25% Carbographite
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Density 2.04 - 2.10 g/cc
0.0737 - 0.0759 lb/in³
extruded; ASTM D792
Guarniflon PTFE G415 Polytetrafluoroethylene 25% Soft Carbon
PTFE G Standard Compound with carbon..Properties: Good thermal and electrical conductivity. Good resistance to deformation. Excellent resistance to load with low coefficient of friction and high ..
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy
E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Density 2.04 g/cc
0.0737 lb/in³
ASTM D792
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy
E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Copyright © lookpolymers.com All Rights Reserved