Polymer Property : Density = 14.95 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 14.95 g/cc
0.5401 lb/in³
Goodfellow Tungsten Carbide/Cobalt
Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard cerami..
Density 14.95 g/cc
0.5401 lb/in³
CoorsTek ACI-Ni6 Tungsten Carbide
Applications: seal rings, plungers, liners, nozzles, valve components, pump components, wear components in the oil & gas, construction, and agriculture equipment industries
Density 14.95 g/cc
0.5401 lb/in³
China Tungsten YG6 Tungsten Carbide
Information provided by China Tungsten
Density 14.95 g/cc
0.5401 lb/in³
China Tungsten YG6A Tungsten Carbide
Information provided by China Tungsten
Density 14.95 g/cc
0.5401 lb/in³
China Tungsten YG6C Tungsten Carbide
Information provided by China Tungsten