Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 11.02 g/cc | 0.3981 lb/in³ | |
Indium Corp. Indalloy® 151 Pb-Sn-Ag Solder Alloy Similar to Indalloy #165 (Standard lead-silver-tin eutectic solder with wide application in semiconductor assembly.)Information provided by the manufacturer, Indium Corporation. |
|||
Density | 11.02 g/cc | 0.3981 lb/in³ | |
Indium Corp. Indalloy® 164 Pb-In-Ag Solder Alloy This alloy is very useful in the 300°C range. It has particularly good thermal fatigue properties as well as the minimal gold leaching properties of indium-lead alloys. Often used in reducing atm.. |
|||
Density | 11.02 g/cc | 0.3981 lb/in³ | |
Williams Advanced Alloys WS296 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 11.02 g/cc | 0.3981 lb/in³ | |
Williams Advanced Alloys WS300 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |