Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 11.0 g/cc | 0.397 lb/in³ | ISO 1183 |
PolyOne Trilliant™ HC HC6200-5001 XR Grey Polyamide 12 (Nylon 12) The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead.. |
|||
Density | >= 11.0 g/cc | >= 0.397 lb/in³ | |
Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection weld.. |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Indium Corp. Indalloy 155 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Density | >= 11.0 g/cc | >= 0.397 lb/in³ | |
Mi-Tech Metals TC50 50 Tungsten Carbide/50 Copper PM Metal Composite Mi-Tech refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Used for light duty projection welding die.. |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Indium Corp. Indalloy 12 Lead Solder Alloy Tin-free indium solderInformation Provided by Indium Corporation |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PH1100B PA 6 LNP* THERMOCOMP* PH1100B is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity Filler. Added features of this material include: High Specific Gravity. |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Wieland 1103 Wilaform Gold Hard yellow gold alloy particularly suitable for decoration casting.Applications: casting, laminar decorationDental |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Wieland 1114 Wilaform Gold Hard yellow gold alloy with good extensibility. Universally applicable in decoration manufacturing.Applications: casting, chains, coin/shape, laminar decoration, pipes, tubingDental |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Wieland 1751 Wilaform Palladium Approach-steady palladium alloy for nearly all purposes in decoration manufacturingApplications: casting, chains, laminar decoration, pipes, tubingDental |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Williams Advanced Alloys WS292 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
Williams Advanced Alloys WS310 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
CMW® ELKONIUM 28 Silver Alloy ELKONIUM® 28, a silver-manganese alloy, was developed by CMW specifically for the control of the transfer of contact material in low voltage DC applications. It is used as a positive contact operat.. |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | |
LATI Latimass 82-03 D110 PA12 Specific density compound based on Polyamide 12 (PA12). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 11.0 g/cc | 0.397 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA12 1100 Tungsten Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Tungsten FillerInformation provided by TP Composites, Inc. |