Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.311 g/cc | 0.04736 lb/in³ | |
CRP Technology Windform® LX 2.0 Polyamide Composite Processed by selective laser sintering (SLS). Windform® LX 2.0 has improved the already excellent performances of Windform® LX and this can be noticed from technical properties and sinterability .. |