Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.992 g/cc | 0.0358 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 8502 EXCEL GREY Heating aging the material 1000 hours at 125°C leads to a +7% change in the tensile strength, +4% change in elongation, and +12% change in tear strength. Ash is 16%. Multi-Flex TPE contains Krato.. |
|||
Density | 0.992 g/cc | 0.0358 lb/in³ | |
NEU NeuSoft™ 455-50A Ester/ether TPU / SBC blend |
|||
Density | 0.992 - 1.44 g/cc | 0.0358 - 0.0520 lb/in³ | Average value: 1.21 g/cc Grade Count:211 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Density | 0.992 g/cc | 0.0358 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Catalyst CT/4 BLK Polyolefin Catalyst CT/4 BLK is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Coge.. |