Material Notes:
Catalyst CT/4 BLK is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Cogegum® GFR series compounds, it contains a special carbon black grade to impart fair UV/VIS resistance. Catalyst CT/4 BLK can be used in a wide application range due to its catalytic activity and the anti-ageing effect given to the final product. It contains also a metal deactivator that allows its use also in direct contact with untinned copperFeatures: Copper Contact Stabilized; Halogen FreeUses: Wire & Cable ApplicationsInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 0.992 g/cc
0.0358 lb/in³
ASTM D792
Apparent Bulk Density 0.600 g/cc
0.0217 lb/in³
ASTM D1895
Carbon Black Loading >= 10 %
>= 10 %
ASTM D1603
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
North America
Color Black
RoHS Compliance RoHS Compliant