Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.978 g/cc | 0.0353 lb/in³ | |
NEU NeuSoft™ 597-50A Industrial Ether TPU / SBC blend |
|||
Density | 0.978 g/cc | 0.0353 lb/in³ | ASTM D792 |
North Wood Plastics 60 PP + UNIFILL (20% Wood Fiber) Data provided by North Wood Plastics, Inc. UNIFILL-60 is a general purpose polyolefin compound compatible in both PP and HDPE. It is a masterbatch with 60% high quality pine wood flour filler. It.. |
|||
Density | 0.978 g/cc @Temperature 20.0 °C |
0.0353 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell Glycol Ether DBA Diethylene glycol butyl ether acetate Information provided by Lyondell. |
|||
Density | 0.978 g/cc @Temperature 15.6 °C |
0.0353 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil Exterex™ TM111 Synthetic Fluid Product Description: Esterex™ Tirmellitate Esters are API category Group V fluids. These esters have excellent low-temperature properties, good lubricating properties and low volatilities. Esterex™.. |
|||
Density | 0.978 - 1.11 g/cc | 0.0353 - 0.0401 lb/in³ | Average value: 1.05 g/cc Grade Count:9 |
Overview of materials for Silicone Polyurethane, Ether Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Ether Based". Each property range of values reported is minimum and maximum value.. |