Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.918 g/cc | 0.0332 lb/in³ | load density; ASTM D1505 |
SABIC 218B Linear Low Density Polyethylene for Cast Film Product Description: 218B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | load density; ASTM D1505 |
SABIC 318B Linear Low Density Polyethylene for Cast Film Product Description: 318B is a Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high processing temperatures u.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | load density; ASTM D1505 |
SABIC 6318B Linear Low Density Polyethylene for Cast Film Product Description: 6318B is a hexene copolymer Linear Low Density Polyethylene grade designed to provide easy processability and specially formulated for optimum thermal stability at high process.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Reliance Industries Reclair F22020 Polyethylene Butene comonomer based Linear Low Density Polyethylene blow film grade. Reclair F22020 has optimum levels of antioxidants, antiblocking agents, and slip additives. Applications:general purpose, and.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 102-15 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 107-18 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-15 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 - 0.924 g/cc | 0.0332 - 0.0334 lb/in³ | |
Kazanorgsintez 153-21 Composition of Low Density Polyethylene, Crack-Proof Production Method: Composition is achieved on the basis of grades 10204-003, 15303-003, 10703-020 and formulas of additives 15, 16, 17, 18, 19, 20, 21, 22, and 23. Application: Intended for prod.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake EC800AA Low Density Polyethylene WESTLAKE low-density polyethylene EC800 is a general-purpose low-density formulation used for extrusion coating applications.Application/UsesGeneral extrusion coatingFDA: This material complies with.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake LF2040 Hexene Linear Low Density Polyethylene Westlake LF2040 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® D139 m-LLDPE Linear Low Density Polyethylene Low Density PolyethyleneCustomer Benefits: Possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved processability (bubble stability, down-.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1018KA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1018LA Metallocene Polyethylene Resin (Asia Pacific Grade) Product Description: Exceed 1018 resins are a metallocene ethylene-hexene copolymer. Films made of Exceed 1018 resins have outstanding tensile, impact strength and puncture. These superior propertie.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
ExxonMobil LL 1001x76 Blown Film Resin LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1001.32 Linear Low Density Polyethylene Resin Product Description: LL 1001.32 is a butane LLDPE resin. Films made from LL 1001.32 have very good tensile and toughness properties.Availability: Latin America, North America and South America Addit.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil LLDPE LL 3003.39 Linear Low Density Polyethylene Resin Product Description: LL 3003 is a hexane copolymer LLDPE film resin. Films made from LL 3003 resins have outstanding tensile properties, as well as stiffness and toughness. These superior strength p.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018HA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018HA have outstanding tensile, impact strength and puncture. These superior strength proper.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D792 |
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Braskem LH 218 LLDPE Cast Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Stretch film; shrink film; "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Braskem LL 118/21 LLDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Bapolene® 122F Polyethylene, Film Grade Bapolene LL122F is a general purpose LLDPE for blown film extrusion applications. This resin offers excellent tensile and toughness properties. Contains medium levels of slip/antiblock additives. .. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Huntsman Rexell® L2101 Injection Molding LLDPE
(discontinued **) Linear-low very low density copolymer, injection molding, FDA compliant.Features: High flow, flexible with excellent environmental stress crack (ESCR), and warpage resistance.Applications: Fitments,.. |
|||
Density | 0.918 - 0.955 g/cc | 0.0332 - 0.0345 lb/in³ | Average value: 0.923 g/cc Grade Count:39 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Lushan M-10F Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
ExxonMobil Exceed™ 1018 EB Blown Film Resin
(discontinued **) Exceed 1018 resins are hexene copolymer produced using ExxonMobil Chemicals Exxpol® Technology. Films made from 1018 resins have outstanding tensile properties and impact and puncture toughness. .. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1018CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1018 CA is a metallocene ethylene-hexene copolymers. Films are made of Exceed 1018CA have outstanding tensile, puncture resistance and very good sealing properties. These.. |
|||
Density | 0.918 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 7109CL LLDPE Blown Film Resin