Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 500P Polypropylene Homopolymer for Raffia Applications Product Description: PP 500P is specially developed for producing stretched tapes with the following features:Consistent processabilityEasy orientationLow water carry overGood mechanical properties.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 513MN40 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 513MN40 is a controlled rheology PP grade of narrow molecular weight distribution. It contains an antistatic agent and is especially developed for producing injection molde.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 5701P Polypropylene Homopolymer for Injection Molding Product Description: PP 5701P is specially for producing rigid injection molded articles for general purpose applications. It gives consistent processability and high gloss in the products.Typical.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 5707N Polypropylene Homopolymer STIFFPACT for Injection Molding Product Description: PP 5707N is a reactor PP homopolymer grade with antistatic and nucleated agents. It is suitable for producing injection molded applications and gives consistent processability.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 25-0110 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
Network Polymers NPP 25-2003 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
SABIC PP 57MNK10 Polypropylene Impact Copolymer for Injection Molding Product Description: PP 57MNK10 is a controlled rheology PP grade of medium molecular weight distribution specially developed for producing injection molded articles. This grade has an excellent i.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
M. Holland Company PP720 Polypropylene Homopolymer Gas-fading resistantHomopolymerGood processabilityGood UV resistanceApplications: FabricsSpunbond non-wovensYarn |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | |
Silon Tabond 5009 Adhesive Resin Tabond 5009 is a chemically modified Polypropylene. This grade is for coextrusion coating of multilayer film to give adhesion between the layers.Characteristics: • Strong adhesion to Aluminium .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis BF330MO Polypropylene Copolymer BF330MO is a heterophasic copolymer. This polymer is characterized by an optimum combination of high stiffness, high impact strength and good flow properties. This grade is designed for high-speed i.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Bormed™ RE806CF Polypropylene Random Copolymer Bormed™ RE806CF is a random copolymer. The material is specially formulated for medical applications. Applications: Bormed™ RE806CF is recommended for medical packaging. Bormed™ RE806CF contai.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Borpact™ BC918CF Polypropylene Copolymer Borpact™ BC918CF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. Optical properties will not be deteriorated as with conventional homo or .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Borpact™ SG910MO Polypropylene for Injection Molding Borpact™ SG910MO is a high impact and transparent polypropylene. This grade provides high gloss, high transparency and excellent impact properties. Applications: containers and products with medium.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis BorPURE™ RE450MO Polypropylene Random Copolymer BorPure™ RE450MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is characterized by optimum combination of high impact strength and.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Daplen™ KSR4525 Polypropylene Reactor Elastomer Modified Daplen KSR4525 is a reactor elastomer modified polypropylene intended for injection molding. Daplean KSR4525 is a material with excellent impact/stiffness ratio. The grade is available in natural .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis HC600TF Polypropylene HC600TF is a polypropylene homopolymer intended for thermoformed packaging applications. Its very good organoleptic properties allows this grade to be used with any masterbatch without discoloring .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis HK060AE Polypropylene Homopolymer HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPH 3060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 3060 is homopolymer.ApplicationATOFINA Polypropylene PPH 3060 is characterized by a low fluidity for continuous extrusion of strapping, rope fibers and high tenacity tapes .. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Total PPH 3371 Polypropylene, Oriented Film Extrusion Grade Homopolymer film gradeLow Residuals - Fina 3371 utilizes the new Fina proprietary process technology to provide extremely low residuals for improved color stability and clarity.Slip/Antiblock - Fina.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Total PPH 3620WZ Polypropylene, Injection Molding Grade Injection molding homopolymerNucleation - FINA 3620WZ is engineered with nucleation to provide fast cycle time and improve contact clarity in thin wall multi- cavity molds.Antistat - FINA 3620WZ con.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Total PPH 3721WZ Polypropylene, Injection Molding Grade High flow reactor homopolymer with a high level of antistatHigh Flow - FINA 3721WZ is designed with high flow characteristics for ease of filling thin wall parts.High Antistat - FINA 3721WZ is engin.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Total PPH 3860X Polypropylene, Extrusion Grade High flow reactor grade homopolymer for nonwoven fibersHigh Purity - FINA 3860X features extremely high purity for processing in micro denier fibers.FDA - FINA 3860X complies with all applicable FDA.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Total PPH 3925WZ Polypropylene, Injection Molding Grade Easy flow injection molding homopolymerNucleation - FINA 3925WZ is nucleated to provide fast cycle time and improve contact clarity.Antistat - FINA 3925WZ contains an antistat that will help protect.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Bormed™ RD808CF Polypropylene Random Copolymer Bormed™ RD808CF is a random copolymer. Applications: Bormed™ RD808CF is intended for packaging for medical devices, thin pouches, and packaging for pharmaceutical products. Additives: Bormed™ R.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Total PPC 4640 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4640 is a nucleated copolymer. PPC 4640 is characterized by good stiffness and impact resistance coupled with high creep resistance. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792A |
Braskem H 503 Injection Molding Polypropylene Description: H 503 is a low melt flow rate additivated homopolyme used for general purposes. It is designed for injection molding, raffia extrusion, bioriented film and general extrusion. This produ.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D1505 |
Amco PRIMATOP PP HOMO 038X Fiber Grade Polypropylene PP HOMO 038X features low water carryover. Applications include woven fabric and bags, rope and cordage, woven carpet backing, and woven geotextile fabrics.Former A-Top Polymers product; part of Amc.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792 |
Plastics Group Polifil® RP-PP Polypropylene, Molding Grade Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ISO 1183 |
Borealis Bormod™ HC904CF Polypropylene Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tech.. |
|||
Density | 0.905 g/cc | 0.0327 lb/in³ | ASTM D792A |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |