Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | Average value: 0.903 g/cc Grade Count:89 |
Overview of materials for Polypropylene, Fiber Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Fiber Grade". Each property range of values reported is minimum and maximum values of app.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13G-00 Polypropylene Homopolymer
(discontinued **) Formerly Amoco® 7444. Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Rigid packaging, Medical componentsComplies with FDA specification, Title 21, C.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7556 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: High speed spinning, Improved bulk, Low gas fadeTypical applications: Upholstery, BCF carpet yarnsComplies with FDA specification, Title 21, CF.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7644 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeTypical applications: Consumer products, CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 7942 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Excellent mold release, AntistaticTypical applications: Closures, Thin-walled rigid packagingComplies with FDA specification, Title 21, CFR .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H38G-01 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fadeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.Typical pr.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3243 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purposeComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05A-00 Polypropylene Homopolymer Grade H05A-00 is an antistatic polypropylene homopolymer for injection molding & extrusion applications. This material meeets the requirements of the U.S. Food and Drug Administration as specified .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05M-00 Polypropylene Homopolymer Grade H05M-00 is a general purpose polypropylene homopolymer for injection molding applications. This resin provides good long-term heat stability. This material meets the requirements of the Food.. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.886 g/cc @Temperature 15.6 °C |
0.0320 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 150 ND Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | ASTM D792 |
Dow FLEXOMER™ DFDA-1098 NT Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1098 NT is an ethylene-butene copolymer with a unique olefinic composition for improved process-ability and material handling. This product is produced via gas phase polymerization .. |
|||
Density | 0.886 g/cc @Temperature 15.0 °C |
0.0320 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil Mobil Pegasus 801 40 Mobil Pegasus 801 is an SAE 40 premium performance gas engine oil intended for the lubrication of all classes of gas engines operating at low, medium and high speeds where low ash or ashless oils ar.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05H-01 Polypropylene Homopolymer Grade H05H-01 is a homopolymer polypropylene for injection molding applications. It is an excellent long-term heat aging grade and offers superior extraction resistance in hot aqueous solutions. T.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H08U-00 Polypropylene Homopolymer, Fiber Grade Suggested fabrication methods: Fiber spinningFeatures: UV stable, High tenacityTypical applications: Geotextiles, Continuous filamentComplies with FDA specification, Title 21, CFR 177.1520.Typical p.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9965 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: NucleatedTypical applications: CompoundingComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H35Z-01 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Rigid packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3541 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: General purpose, High melt flowComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded sam.. |
|||
Density | 0.886 g/cc | 0.0320 lb/in³ | |
BASF 3-Dimethylaminopropane-1-ol Formula: C5H13NOCAS: 3179-63-3Description: 3-Dimethylaminopropane-1-ol is a colorless to yellow liquid with an amine-like odor. It is miscible in water.Synonyms: 1-Propanol, 3-(dimethylamino)- Dime.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H07D-00 Polypropylene Homopolymer Grade H07D-00 is a polypropylene homopolymer for cast film applications that require slip and antiblock additives. This resin meets the requirements of the Food and Drug Administration as specified .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acclear® 8449 Random Copolymer Polypropylene, High Clarity Grade
(discontinued **) Suggested fabrication methods: Injection molding; Stretch blow moldingFeatures: Ultra high clarity, Good impact, Excellent static controlTypical applications: Housewares, Rigid packagingComplies wit.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Accpro® 9117 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Sheet; ExtrusionFeatures: Improved MVTR, Stain resistanceTypical applications: Film, Rigid packagingComplies with FDA specification, Title 21, CFR 177.1520.Typical pro.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H13Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Packaging, Consumer productsComplies with FDA specification, Title 21, CFR 177.1520.Typical prope.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Amoco® 6361 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Extrusion; Blow moldingFeatures: Ease of processingTypical applications: Oriented film, Sheet, Fiber, Profile, Consumer productsComplies with FDA specification, Title .. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H05Z-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticTypical applications: Closures, DispensersComplies with FDA specification, Title 21, CFR 177.1520.Typical property data.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H28U-00 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Radiation stableTypical applications: MedicalComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
Ineos H38K-00 Polypropylene Homopolymer, Fiber Grade
(discontinued **) Suggested fabrication methods: Fiber spinningFeatures: Very high speed spinning, Low gas fade, Low smokeTypical applications: Spunbound fabricsComplies with FDA specification, Title 21, CFR 177.1520.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3434 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High gloss, Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded s.. |
|||
Density | 0.886 - 0.926 g/cc | 0.0320 - 0.0335 lb/in³ | ASTM D1505 |
BP Amoco Acctuf® 3638 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: Compounding, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples. |