Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2315 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance of heat resistance, flexibility and stiffness, good wetting, and medium open timeApplications: Component.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2730 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Very low softening point, medium viscosity, good track, and very long open timeApplications: Component of hot me.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 3280 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: Temperature resistance, high melt viscosity, and hardnessApplications: Component of modified bitumen roofing.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4730 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Butene-1 copolymer and FDA compliantFeatures: Excellent low temperature flexibility, lower processing temperature, and superior adhesionApplications: Flooding and f.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 1215 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Good heat resistance, short open time, and excellent wetting propertiesApplications: Lamination of reinforced tapes and prot.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 1330 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Medium open timeApplications: Lamination of reinforced tapes and protective overwrapsOther Properties: Ring and Ball Softeni.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2115 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point and short open timeApplications: Component of hot melt adhesives, sealants and specialty.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 2180 Amorphous Polyalphaolefin (APAO) Adhesive and Sealant Grade.Description: Propylene homopolymer and FDA compliantFeatures: High softening point, short open time, good cohesive strength, and high viscosityApplications: Component of h.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4330 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Moisture barrier and adhesionApplications: Flooding and filling compounds for wire and cableOther Properties: Ring and.. |
|||
Density | 0.860 - 2.60 g/cc | 0.0311 - 0.0939 lb/in³ | Average value: 1.34 g/cc Grade Count:114 |
Overview of materials for Epoxy Cure Resin This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Cure Resin". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Density | 0.860 - 0.940 g/cc | 0.0311 - 0.0340 lb/in³ | Apparent |
Gouda Vuurvast GI 28 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Medium Mobil DTE Oil Named Series The Mobil DTE Oil Named Series of lubricants are premium performance circulating lubricants designed for applications including steam and hydro turbine sets and other systems where long lubricant se.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 3430 EPDM Hydrocarbon Rubber Description: This amorphous, very low diene containing ethylenepropylene terpolymer (EPDM) is suitable for peroxide cured articles. Nordel® IP 3430 can also be blended with butyl rubber to improve .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 3670 EPDM Hydrocarbon Rubber Description: Slightly crystalline, ethylene-propylene-diene (EPDM) terpolymer designed for calendering; offers excellent processing characteristics. Low unsaturation level provides stability during .. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 4520 EPDM Hydrocarbon Rubber Description: Nordel® IP 4520 is an amorphous EPDM grade designed for molded applications. It is ideally suited for injection and transfer molded brake parts, corner moldings, general purpose gasket.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D297 |
Dow Nordel® IP 4640 EPDM Hydrocarbon Rubber Description: Nordel® IP 4640 is an amorphous EPDM grade designed for molded and extruded applications. It is ideally suited for general-purpose gaskets and moldings, extruded profiles and hoses. Th.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 32 AW Turbine Oil Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear Diamond Class® 32 Turbine Oil Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear® 32 Multipurpose R&O Oil Description: Conoco Hydroclear Multipurpose R&O Oil is a rust- and oxidation inhibited industrial oil with ashless wear protection formulated from premium Conoco hydrocracked base stocks. Hydroclear.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
ConocoPhillips Hydroclear® 32 Turbine Oil Description: Conoco Hydroclear Turbine Oil is a premium rust- and oxidationinhibited turbine oil formulated from exclusive Conoco hydrocracked base stock. Hydroclear Turbine Oil is specially formula.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | |
BASF 1,2-PDA 1,2-Propylenediamine Formula: C3H10N2CAS: 78-90-0Description: 1,2-Propylenediamine is a colorless liquid, with an amine-like odor. It is also miscible with water in all proportionsSynonyms: 1,2-PDA, 1,2-Propanediamine,.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ExxonMobil Method |
ExxonMobil EXXELOR™ VA 1803 Maleic anhydride functionalized elastomeric ethylene copolymer Product Description: Exxelor VA 1803 polymer resin is a high flow, amorphous ethylene copolymer functionalized with maleic anhydride by reactive extrusion. Its fully saturated backbone results in ou.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 4535 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Excellent low temperature flexibility, moisture barrier and adhesionApplications: Flooding and filling compounds for w.. |
|||
Density | 0.860 g/cc @Temperature 15.0 °C |
0.0311 lb/in³ @Temperature 59.0 °F |
ASTM D1298 |
ExxonMobil 798 Mobil DTE 790 Series Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 1315 Amorphous Polyalphaolefin (APAO) Laminate Grade.Description: Ethylene copolymer and FDA compliantFeatures: Medium open timeApplications: Lamination of reinforced tapes and protective overwrapsOther Properties: Ring and Ball Softeni.. |
|||
Density | 0.860 g/cc | 0.0311 lb/in³ | ASTM D 792 |
REXtac Rextac® RT 5219 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: High molecular weight REXtac, ethylene copolymer, and FDA compliantFeatures: High ethylene level and low crystallinityApplications: Component of modified .. |