Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Pyrotek A-1/S-1 Tadpoles A-1 glass fiber core with highly abrasion-resistant S-1 fabric jacket and mounting flange.AdvantagesExcellent Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Pyrotek A-1/Z-5 Tadpoles A-1 rope core with jacket and mounting flange of densely woven glass cloth or wire reinforced glass cloth.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrot.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Pyrotek A-1 Glass Fiber Core Rope Compressible, inexpensive rope. Glass fiber core with heavy gauge glass fabric jacket. Loses tensile strength after 340°C but remains intact.AdvantagesGood Abrasion Resistance Good Compression an.. |
|||
Density | 0.800 - 2.33 g/cc | 0.0289 - 0.0842 lb/in³ | Average value: 1.30 g/cc Grade Count:100 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-1 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-13 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-16 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-17 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-18 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-3 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
MarkeTech Carbon Aerogel Data provided by the supplier, MarkeTech International.Availability: Paper Sheets: 85 x 250 mm; Random Pieces 0.5-20 mm; Granules and Powder.Resorcinol Formaldehyde and Silica Aerogels are also list.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ M DM-650A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 95Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Density | >= 0.800 g/cc @Temperature 20.0 °C |
>= 0.0289 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-9 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ F DF-235A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 80Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Solvay Chemicals CASO® FEED POWDER Calcium Chloride Solvay is manufacturing and placing on the market dihydrate calcium chloride (CASO®FEED), feed material of mineral origin in conformity with European Directive 2002/32/EU and its amendments on u.. |
|||
Density | 0.800 - 0.900 g/cc | 0.0289 - 0.0325 lb/in³ | |
Solvay Chemicals CASO® FOOD FLAKES Food additive E 509, Calcium Chloride CASO® FOOD Flakes, is a dihydrate calcium chloride food grade of mineral origin. In the context of the European Regulation N° 1333/2008 on food additives, permitted for use in foodstuffs, and .. |
|||
Density | <= 0.800 g/cc @Temperature 0.900 °C |
<= 0.0289 lb/in³ @Temperature 33.6 °F |
|
Solvay Chemicals CASO® SIEVED FLAKES Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - .. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
SPHERE ONE EXTENDOSPHERESâ„¢ 300/600 Hollow Spheres EXTENDOSPHERESâ„¢300/600 are efficient, lightweight additives for most resin systems. When Extendospheresâ„¢ replace heavier, more expensive components on an equivalent volume basis, they can .. |
|||
Density | <= 0.800 g/cc @Temperature 0.900 °C |
<= 0.0289 lb/in³ @Temperature 33.6 °F |
|
Solvay Chemicals CASO® TECHNICAL FLAKES Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10035-04-8/ EINECS - .. |
|||
Density | 0.800 - 0.840 g/cc @Temperature 15.0 °C |
0.0289 - 0.0303 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Grade 2 Diesel Oil Diesel oils are a mix of liquid hydrocarbons obtained from crude oil through distillation and hydrogenation refining, usually boiling within to 370°C. They may contain additives to improve their ap.. |
|||
Density | 0.800 g/cc @Temperature 15.0 °C |
0.0289 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil 1 5W-30 Mobil 1 5W-30 is a high performance fully synthetic engine oil designed to exceed the industry`s toughest standards and outperform all conventional oils.. Mobil 1 5W-30 is engineered to help keep en.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Zircar Ceramics Z-500 Alumina-Silica Insulation Useful to temperatures of 1000°C (1832°F) Z-500 is uniformly rigidized and hard throughout its entire thickness, requiring no re-rigidizing after precision machining into complex shapes and confia.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Trelleborg Emerson & Cuming Stycast® 1090/11 Two-Component General Purpose Encapsulant Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as .. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | ASTM D1505 |
CPC - Vycom SEABOARD™ LITE High density polyethylene (HDPE) Seaboard Lite is a high density polyethylene (HDPE) sheet formulated to meet the specific requirements of marine and other outdoor environments. Seaboard Lite is UV stable and will withstand the ele.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
DuPont™ Nomex® 410 Paper, 3 mil Nominal Thickness Nomex® Type 410 is a calendared insulation paper which offers high inherent dielectric strength, mechanical toughness, flexibility, and resilience. It is the original form of Nomex® paper and is .. |
|||
Density | 0.800 g/cc @Temperature 15.6 °C |
0.0289 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Varsol™ 140 Naphtha Non-dearomatized Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
3M Scotch-Weld™ AC77 Instant Adhesive Primer 3M™ Scotch-Weld™ Instant Adhesive Primer AC77 is designed for difficult-to-bond, low surface energy plastics such as polypropylene, polyethylene, and PTFE. This primer needs to be applied to each .. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | Foam |
Aptek DI-STRATE 95196 Microwave/RF Foam Substrate DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Auto RadarInformation provided by Aptek Lab.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | oven dried |
Pyrotek Pyrocast PT-60 Castable Refractory Pyrocast PT-60 is a ceramic fiber based insulating castable with very low thermal conductivity and excellent resistance to thermal shock.ApplicationsLaunder linings Distributor pan linings Ladle lin.. |
|||
Density | 0.800 g/cc | 0.0289 lb/in³ | |
Solvay RHODAPHOSE® VDPA (WET CAKE) Phosphorus derivative Identification: VINYLIDENE DIPHOSPHONIC ACID, TETRASODIUM SALT.CAS: 33016 – 77 – 2ELINCS: 443 – 520 – 7Solubility: Soluble in waterAvailable in: Asia Pacific, Europe, Latin America and North Ame.. |