Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.721 g/cc | 0.0260 lb/in³ | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | Dry |
Unifrax Fiberfrax® LDS AL-Moldable Moldable Insulation Fiberfrax LDS and LDS-AL moldables consist of Fiberfrax ceramic fibers dispersed in a sticky water-based refractory binder. These materials have a putty-like consistency which permits application b.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
Zircar Zirconia M-45 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
CMT Materials HYTAC® XTL Tough Thermoplastic Syntactic Foam HYTAC®-XTL was developed to offer an improved surface quality after machining when compared to our popular HYTAC-B1X. This is particularly important when working with sticky or transparent plastic.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | ASTM C134 |
BNZ Materials BNZ-25 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | ASTM D1056 |
ACC Magnifoam™ MFSILTEC™-HD MTI Silicones Silicone Foam Part of the Amber Chemical Group. Data provided by manufacturer. |
|||
Density | >= 0.721 g/cc | >= 0.0260 lb/in³ | |
Monmouth Rubber & Plastics Superbounce 90 NEO/SBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
Pyrotek Wollite 45 Insulating Castable Wollite material is a solid, light weight mineral foam which is stable during its preparation and during subsequent curing and drying. Because of the foam properties it is well suited for casting c.. |
|||
Density | 0.721 g/cc | 0.0260 lb/in³ | |
BNZ Materials 2645LI Insulating Aggregate BNZ manufactures a variety of insulating and dense castable refractories to meet the exacting needs of the high temperature processing industries. These hydraulic setting products are suitable for i.. |