Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.640 g/cc | 0.0231 lb/in³ | |
Pyrotek A-2 Fiberglass Rope An A-1 substitute fiberglass rope.AdvantagesGood Abrasion Resistance Good Compression and Recall Information provided by Pyrotek. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
Pyrotek Pyrocast L-30 Moldable Refractory Pyrocast L-30 is a refractory moldable designed for use in contact with molten aluminum. Pyrocast L-30 has excellent workability for use as an insulating lining or patching material and is recommen.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ F DF-225A Closed Cell Foam Polyurethane TDI backbone: ester.Shore 00 Hardness: 70Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ F DF-640A Closed Cell Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ M DM-640A Foam Polyurethane MDI backbone: ester.Shore 00 Hardness: 85Summary: Durethane M is a flexible, microcellular, open cell and closed cell urethane foam. Because it is mechanically mixed, the cell size is uniform. Dur.. |
|||
Density | 0.640 - 0.700 g/cc | 0.0231 - 0.0253 lb/in³ | Apparent |
Gouda Vuurvast GI 23 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 40 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
Zircar Ceramics NKO Castertip Main stay "low mass hard tip" used on all makes of continuous thin strip aluminum casting equipment. NKO is a rigid combination of refractory ceramic fiber and inorganic binders. Information provid.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
Zircar Refractory Composites RS-SI SILICA MOLDABLE ZIRCAR Silica Moldable Type RS-SI Moldable is a wet blanket that is a combination of high purity amorphous silica fibers and inorganic silica binder. The fibers are 6-9 um in diameter and are consid.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D792 |
Covestro Baydur® 660 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D792 |
Covestro Baydur® 726 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | ASTM D792 |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 40 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | helium pycnometer |
CRG Industries Advantic™ 40 Syntactic Foam Advantic is a series of lightweight, engineered foams consisting of manufactured glass, polymer, or ceramic hollow spheres embedded in a resin matrix, such as epoxy or cyanate ester. CRG Industries’.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M Bumpon™ SJ5208 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M Bumpon™ SJ5216 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M Bumpon™ SJ5904 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M Bumpon™ SJ5908 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M SJ5201 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Density | 0.640 g/cc | 0.0231 lb/in³ | |
3M SJ5202 Protective Product, Die Cut Shapes 3M Bumpon Protective Products SJ5201 and SJ5202 are pressure-sensitive, adhesive backed polyurethane products made from SJ5200 Series soft foam rollstock. A hexagon shape is often preferred for vari.. |