Physical Properties Metric English Comments
Density 0.230 g/cc
0.00831 lb/in³
Effective Density as measured by liquid displacement
Potters Industries Q-Cel® 7023S Hollow Engineered Glass Microspheres
Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me..
Density 0.230 g/cc
0.00831 lb/in³
Zircar Ceramics MICROSIL Microporous Insulation
MICROSIL Microporous Insulation is an insulation material. Having thermal conductivity an order of magnitude lower than ceramic fiber materials Microsil Microporous Insulation can be an integral par..
Density 0.230 g/cc
0.00831 lb/in³
foam with adhesive; ASTM D3574
3M 4726 Single-Coated Foam Tape
3M™ Single-Coated Foam Tapes will adhere to a variety of substrates, including latex-painted wood, lacquered wood, enameled steel, glass, aluminum, stainless steel, acrylic, ABS, and PVC (non-plast..
Density 0.230 - 0.250 g/cc
0.00831 - 0.00903 lb/in³
Free Density
C.O.I.M. UREXTER® T 400 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Density 0.230 g/cc
0.00831 lb/in³
3M XLD3000 Glass Bubbles
3M™ Glass Bubbles XLD3000 are high-strength additives for polymers made from a water-resistant and chemically stable soda-lime-borosilicate glass. These hollow glass bubbles can be compounded with ..
Density 0.230 - 0.270 g/cc
0.00831 - 0.00975 lb/in³
3M K25 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.230 - 0.270 g/cc
0.00831 - 0.00975 lb/in³
ISO 845-88
Eurofoam Porocell 251 GR NBR/PVC Foam
Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof..