Physical Properties Metric English Comments
Density 0.210 g/cc
0.00759 lb/in³
Effective density of spheres
Potters Industries Q-Cel® 300
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Density 0.210 g/cc
0.00759 lb/in³
Pyrotek Fiberseal Paper C-6 Ceramic fiber paper
C-6 is an economical, high strength, Fiberseal paper composed of ceramic fibers, inert fillers and fiberglass.ApplicationsGaskets Seals Linings AdvantagesLow shrinkage Good dielectric properties Uni..
Density 0.210 g/cc
0.00759 lb/in³
Pour Density; ASTM D1513
TIMCAL ENSACO™ 210G Conductive Carbon Black
ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can..
Density 0.210 - 0.250 g/cc
0.00759 - 0.00903 lb/in³
ISO 845-88
Eurofoam Porocell POR 446 NDN NR-SBR Foam
Natural and styrene butadiene rubber foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.210 - 0.290 g/cc
0.00759 - 0.0105 lb/in³
ISO 845-88
Eurofoam Siliconcell SIL 411 Silicone Foam Sheet
Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l.
Density 0.210 - 0.230 g/cc
0.00759 - 0.00831 lb/in³
Free Density
C.O.I.M. UREXTER® F 3 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Density 0.210 g/cc
0.00759 lb/in³
average; ISO 845
3A Composites Core Materials AIREX® T90.210 Easy Processing Structural FST Foam
AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has good mechanical properties and resistance to fatigue, is chemic..
Density 0.210 g/cc
0.00759 lb/in³
average; ISO 845
3A Composites Core Materials AIREX® T92.200 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable, UV r..
Density 0.210 g/cc
0.00759 lb/in³
Pyrotek M-12 Compressible/Insulating Boards
ApplicationsHigh temperature gaskets Furnace covers Trough lining AdvantagesLow density Good insulating ability Information provided by Pyrotek.
Density 0.210 - 1.50 g/cc
0.00759 - 0.0542 lb/in³
Average value: 1.17 g/cc Grade Count:125
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and ..
Copyright © lookpolymers.com All Rights Reserved