Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0900 g/cc | 0.00325 lb/in³ | 2.7 minute residence time pre-expander |
Jackon JACKOCELL® S232 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThis is the low pentane version for densities above 25-30 kg/m3. A substantial reduced pentane emission has been made possible with S232 which will lead the industry in.. |
|||
Density | 0.0900 g/cc | 0.00325 lb/in³ | |
Zircar Refractory Composites RSBL-SOL6 Silica-Magnesia Blanket ZIRCAR Refractory Composites, Inc. insulating blankets are non woven, inorganic, fiber-based products that contain no asbestos. They are engineered for use as thermal barrier materials in high tempe.. |
|||
Density | 0.0900 - 0.125 g/cc | 0.00325 - 0.00452 lb/in³ | sheet density |
Zotefoams Plastazote® HD115 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Density | 0.0900 g/cc | 0.00325 lb/in³ | ISO 845 |
BASF Neopolen® P 9255 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea.. |
|||
Density | 0.0900 g/cc | 0.00325 lb/in³ | ISO 845 |
BASF Neopolen® P 9270 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Density | 0.0900 g/cc | 0.00325 lb/in³ | ISO 845 |
BASF Neopolen® P 9280 0.09 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Density | 0.0900 - 0.115 g/cc | 0.00325 - 0.00415 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® C70.90 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible .. |
|||
Density | 0.0900 g/cc | 0.00325 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® R63.80 Damage Tolerant Foam AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable.. |
|||
Density | 0.0900 - 0.110 g/cc | 0.00325 - 0.00397 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |