Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0650 g/cc | 0.00235 lb/in³ | |
Sharadaa Ceramics MMTCL Ceramics Fiber Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.0650 g/cc | 0.00235 lb/in³ | Nominal skin/skin; BS ISO 7214 1998 |
Zotefoams Evazote® VA65 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0650 g/cc | 0.00235 lb/in³ | average; ISO 845 |
3A Composites Core Materials AIREX® T90.60 Easy Processing Structural FST Foam AIREX® T90 is a closed-cell, thermoplastic and recyclable polymer foam with excellent fire, smoke & toxicity (FST) properties. It has very good mechanical properties and a good resistance to fatigu.. |