Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0641 - 0.128 g/cc | 0.00231 - 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK1111 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.0641 - 0.128 g/cc | 0.00231 - 0.00463 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ DK2121 NEO/EPDM Polymeric Blend Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator Fiberfrax Durablanket HP-S insulation is a needled blanket made from spun Fiberfrax ceramic fibers. Durablanket HP-S insulation combines all of the physical characteristics offered by Durablanket S.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 1/4 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/16 - 4.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-327 - 3/8 - 4.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-36 - 1/8 - 4.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRP - 3/16 - 4.0 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Unifrax Fiberfrax® Duraback® Ceramic Fiber Insulator Fiberfrax Duraback blanket is a strong, lightweight, flexible needled blanket intended for use as a cost-effective back-up insulation in Fiberwall® furnace linings. It is recommended for use up to.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | Available |
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator Fiberfrax Durablanket S insulation is a strong, lightweight, flexible needled blanket that is made from spun ceramic fibers. Available in a wide variety of thicknesses, widths and densities, Durabl.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 1/8- 4.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Hexcel® HexWeb® HRH-10/OX - 3/16 - 4.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | |
Monmouth Rubber & Plastics Durafoam™ C19XLDS EPDM Special Features: Extremely soft and conforms easily to irregular surfaces Superior buoyancy Excellent chemical resistance 100% free of HCFC & CFC Available in custom colors upon request for quoteCo.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | Free Rise Density |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |
|||
Density | 0.0641 g/cc | 0.00231 lb/in³ | ASTM D3575 |
Monmouth Rubber & Plastics Durafoam™ PMR 150 EPDM Performance Features: Softness, stiffness & density infinitely variable.High Ozone Resistance. High Ultraviolet Resistance. Non-Staining. Made from Heat Resistant EPDM Non-fogging (plasticizer free.. |