Material Notes:
C5/C9 type (piperylene and dicyclopentadiene precursor). Has improved compatibility with SBR and EVA; suitable for adhesive tapes and hot-melt adhesives.Information provided by Zeon Chemicals L.P.
Physical Properties Metric English Comments
Brookfield Viscosity 150 cP

@Temperature 200 °C
150 cP

@Temperature 392 °F
Melt
Molecular Weight 1.10e+6 g/mol
1.10e+6 g/mol
Thermal Properties Metric English Comments
Softening Point 99.0 °C
210 °F
Optical Properties Metric English Comments
Gardner Color Number 4.0
4.0
50% in toluene
Chemical Properties Metric English Comments
Acid Value <= 0.10
<= 0.10
mg KOH/g