Zeon Chemicals Hydrin® T3000LL Polyepichlorohydrin Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Hydrin®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Zeon Chemicals Hydrin® T3000LL Polyepichlorohydrin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Hydrin T3000LL is an ethylene oxide/epichlorohydrin/allyl glycidyl ether terpolymer with high oil, fuel and solvent resistance. Compounds using Hydrin T3000LL typically exhibit excellent low and high temperature properties and can be cured using conventional cure systems such as sulfur/sulfur donor or peroxides. Sufficient antioxidant is added during the manufacturing process for normal aging conditions.Lowest viscosity version of Hydrin T3000 for optimum injection flow.
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
Mooney Viscosity 50 - 64

@Temperature 100 °C
50 - 64

@Temperature 212 °F
(1+4)
Ash <= 1.0 %
<= 1.0 %
Zeon Test #1358
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -43.0 °C
-45.4 °F
Component Elements Properties Metric English Comments
Chlorine, Cl 23.7 - 25.7 %
23.7 - 25.7 %
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Zeon Test #1361
Descriptive Properties Value Comments
AGE Content, % 4.5-5.5