Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Von Roll Isola IMI Varnish 708 Solventless Polyester Varnish for Electrical Insulation

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Solventless Electrical Varnish
Manufacturer Von Roll Isola
Trade Name IMI Varnish
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Von Roll Isola IMI Varnish 708 Solventless Polyester Varnish for Electrical Insulation.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 76°C. Usage Notes: Thixitropic version of 709. High film build, low dissipation factor for VPI application.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 180 °C
356 °F
Electrical Properties Metric English Comments
Dielectric Strength 157 kV/mm
3990 kV/in
Processing Properties Metric English Comments
Processing Temperature 160 °C
320 °F
Suggested baking time at this temperature is 1.5 hr.