Material Notes:
Fiberfrax Bulk Fibers are manufactured to be used as feedstock in manufacturing processes or other applications where product consistency is critical. Manufactured on large, computer-controlled furnaces, these products provide customers with consistent material properties. Fiberfrax Bulk Fibers are typically used in the manufacture of other ceramic fiber based product forms such as:High-temperature boards, felts, and papersCombustion chambers for commercial and residential boilersRiser sleeves for molten metal castingFireplace logs and panels for gas fireplacesTap out cones for molten metal applicationsSpecialized vaccum-formed shapesThese bulk fibers can also be directly used as high-temperature fill and packing material in a variety of high-temperature applications, such as:Expansion jointsFurnace base sealsTube sealsBurner tile packingChimney insulationFiberfrax 6000 Series fibers have many of the same properties as the 7000 Series fibers. The main difference is that 6000 Series fibers are manufactured from kaolin clay rather than high-purity alumina-silica raw materials. Since kaolin is a mined material, it may contain impurities such as Fe2O3, TiO2, and Na2O. Even with these impurities, Fiberfrax 6000 Series fibers can provide an effective solution in many vacuum-forming and related applications.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Specific Gravity 2.67 g/cc
2.67 g/cc
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1175 °C
2147 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 45 - 51 %
45 - 51 %
Fe2O3 <= 1.5 %
<= 1.5 %
NaO2 <= 0.50 %
<= 0.50 %
SiO2 46 - 52 %
46 - 52 %
TiO2 <= 2.0 %
<= 2.0 %
Descriptive Properties Value Comments
Average Fiber Diameter (microns) 1.5-2.5
Color Light Gray
Fiber Index (%) 45-55
Temperature Grade (°C) 1260