Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming EP651 Patch Paste

Category Polymer , Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming EP651 Patch Paste.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Density matched brown adhesive for use with EP650 and TB650All information provided by Trelleborg Emerson & Cuming
Physical Properties Metric English Comments
Specific Gravity 1.094 g/cc
1.094 g/cc
ASTM D792
Viscosity 3400 cP

@Temperature 25.0 °C
3400 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
ASTM D2240
Processing Properties Metric English Comments
Pot Life 30 min

@Temperature 25.0 °C
30 min

@Temperature 77.0 °F
Gel Time 210 min

@Temperature 25.0 °C
210 min

@Temperature 77.0 °F
Thin Film
Descriptive Properties Value Comments
Color Brown
Users viewing this material also viewed the following: