Material Notes:
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Plenum Cable Jacketing Agency Ratings: IEC Unspecified Rating; UL QMTT2 .E200337; ICEA Unspecified Rating Processing Method: Extrusion Forms: Pellets Additional Information: Acid Gas, MIL-C-24643: < 5.0 mg Acidity of Gases, IEC-754-2: < 6.0 pH Conductivity: < 2.0 µS/cm Smoke Index, NES-711: < 10.0 Toxicity Index, NES-713: 0.085 Cone Calorimeter at 50 kW/m2, Peak Heat Release Rate: 507 kW/m2 Cone Calorimeter at 50 kW/m2, Total Heat Released: 199 MJ/m2 Cone Calorimeter at 50 kW/m2, Peak Smoke: 2.9 1/m Cone Calorimeter at 50 kW/m2, Time to Sustained Ignition: 88 secInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 38
38
10 seconds; ASTM D2240
Tensile Strength at Break 12.4 MPa
1800 psi
ASTM D638
Elongation at Break 550 %
550 %
ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -46.0 °C
-50.8 °F
ASTM D746
Oxygen Index 35 %
35 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 8.50e+12 ohm-cm
8.50e+12 ohm-cm
ASTM D257
Dielectric Constant 3.52

@Frequency 1000 Hz
3.52

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.0041

@Frequency 1000 Hz
0.0041

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque