Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 40 PHR Polyfil HG90 Filler.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0Zinc Stearate0.5MBTS4.0MBT2.0Thanecure® ZM1.0Sulfur1.5Cumar P1010.0Water Washed Clay - Polyfil HG9040All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 58
>= 58
Tensile Strength, Yield 28.59 MPa
4147 psi
Elongation at Yield 626 %
626 %
100% Modulus 0.00280 GPa
0.406 ksi
200% Modulus 0.00620 GPa
0.899 ksi
300% Modulus 0.009301 GPa
1.349 ksi
Tear Strength 40.6 kN/m
232 pli
Die C
Processing Properties Metric English Comments
Cure Time 16.0 min

@Temperature 68.3 °C
0.267 hour

@Temperature 155 °F
Press cured
Descriptive Properties Value Comments
DIN Abrasion (mm³) 80.5