TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Di-Cup 40C

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Di-Cup 40C.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.FormulationMillathane E34100.0Stearic Acid0.5N220 Black20.0Di-Cup 40C3.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A >= 60
>= 60
Tensile Strength, Yield 19.90 MPa
2886 psi
Elongation at Yield 430 %
430 %
100% Modulus 0.00160 GPa
0.232 ksi
200% Modulus 0.00370 GPa
0.537 ksi
300% Modulus 0.00710 GPa
1.03 ksi