Suqian Unitechem Antioxidant 1010

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Suqian Unitechem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Suqian Unitechem Antioxidant 1010.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Chemical Name: Tetrakis [methylene-3-(3,5-di-tert-butyl-4-hydroxyphenyl-propionate)]methaneCAS NO.: 6683-19-8Molecular Formula: C73H108O12Properties: The product takes on the appearance of white powder, without odor and smell. Soluble in benzene, acetone and chloroform, sparingly soluble in alcohol, insoluble in water. Good extraction-resistance in hot water and low volatility. When used in plastic, the product takes on the best effect of antioxidation.Uses: The product is a kind of phenolic antioxidant. It can be widely used for PE, PP, PC, POM, ABS resin and so on. The amount to be used may be 0.1-0.3%.Information Provided by Suqian Unitechem Co., Ltd.
Physical Properties Metric English Comments
Volatiles <= 0.50 %
<= 0.50 %
Molecular Weight 1178 g/mol
1178 g/mol
Ash <= 0.10 %
<= 0.10 %
Thermal Properties Metric English Comments
Melting Point 110 - 125 °C
230 - 257 °F
Optical Properties Metric English Comments
Transmission, Visible >= 96 %
>= 96 %
425nm
>= 98 %
>= 98 %
500nm
Descriptive Properties Value Comments
Appearance White crystal or powder
Assay (%) >98
effective components