Spartech WJ8341FR-105 PVC and Alloy Products for Wire and Cable

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer Spartech
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Spartech WJ8341FR-105 PVC and Alloy Products for Wire and Cable.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Spartech
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 40.6 °C
105 °F
Descriptive Properties Value Comments
Wire Style electric power and control cables