Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Sulfuric Acid Electrolyte Grade

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Sulfuric Acid Electrolyte Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Sulfuric Acid electrolyte grade is colorless, clear and non-fuming with no visible sediment. It is very corrosive. The 93.2% strength solution complies with the Federal Specification O-S-801F Class 1. Formula: H3SO4 (In aqueous solution)Nomenclature: Sulfuric Acid, Oil of VitriolCAS: 7664-93-9 CAS Index: Sulfuric AcidAvailable in: North AmericaUses: Industrial: Storage batteries and other high quality applicationsInformation provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density >= 1.835 g/cc
>= 0.06629 lb/in³
Thermal Properties Metric English Comments
Melting Point -30.0 °C
-22.0 °F
Freezing Point
Chemical Properties Metric English Comments
Ionic Impurities - Cl (Chloride) <= 10 ppm
<= 10 ppm
Ionic Impurities - Fe (Iron) <= 50 ppm
<= 50 ppm
Descriptive Properties Value Comments
Assay <93.2%
Color 30
APHA
30
Hazen
Composition Ammonium
<10 ppm
Antimony
<1 ppm
Arsenic
<1 ppm
Copper
<50 ppm
Fixed Residue
<0.03%
Manganese
<0.2 ppm
Nickel
<1 ppm
Nitrate
<5 ppm
Selenium
<20 ppm
Sulfurous Acid
<40 ppm
Zinc
<40 ppm
Users viewing this material also viewed the following: