Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer Solvay Specialty Polymers
Trade Name Veradel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® A-704P Polyethersulfone (PESU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Veradel® A-704P (PESU) is a powder designed for dissolving or dispersing into solutions. It can also be ground to smaller particle size, or blended with other solid particles. PESU offers excellent toughness and outstanding hydrolytic resistance. It resists attack from steam, boiling water and mineral acids. Cast films or coatings of PESU are transparent and have additional desirable properties including long term thermal stability, excellent metal adhesion and formability and inherent flame resistance.Features: Acid Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Flow; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Low Molecular Weight; Medium RigidityUses: Adhesives; Coating ApplicationsAdditional Properties: Residual Solvent - Internal Method 0.50 %; Viscosity - Internal Method (40°C): 200 mPa·sInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ISO 62
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.0 µm/m-°C
27.2 µin/in-°F
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Transparent - Slight Yellow
Form Powder
Processing Technique Coating; Solution Processing; Spraying
RoHS Compliance RoHS Compliant