Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer Solvay Specialty Polymers
Trade Name Veradel®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Veradel® 3200P Polyethersulfone (PESU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Veradel® 3000P, 3100P, 3200P, 3400P and 3600P are polyethersulfone (PESU) powders for dissolving or dispersing into solutions. They can also be ground to smaller particle size or blended with other solid particles. The grades differ by their molecular weights, with 3000P the highest and 3600P the lowest. There is a direct correlation between molecular weight and solution viscosity.Features: Acid Resistant; Flame Retardant; Food Contact Acceptable; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium RigidityUses: Adhesives; Coating Applications; Compounding; Film; MembranesAdditional Properties: Residual Solvent - Internal Method 0.50 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.60 %

@Time 86400 sec
0.60 %

@Time 24.0 hour
ISO 62
Viscosity 485 cP
485 cP
Solution Viscosity; ASTM D455
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 49.0 µm/m-°C
27.2 µin/in-°F
Glass Transition Temp, Tg 220 °C
428 °F
ASTM E1356
Compliance Properties Metric English Comments
NSF Yes
Yes
NSF 61
Descriptive Properties Value Comments
Agency Ratings NSF 61
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Transparent - Slight Yellow
Form Granules; Powder
Processing Technique Cast Film; Coating; Solution Processing; Spraying
Users viewing this material also viewed the following: