Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (di

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 30% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH  (di.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good dimensional stability; therefore, typical humid environmental conditions result in only minor changes in the strength and stiffness. This grade of AMODEL resin can withstand the demanding vapor phase and infrared reflow soldering processes typically used in the electronics industry. It is ideally suited for most connectors and electrical devices requiring surface mount technology (SMT). The material offers easy processing using conventional equipment and methods.This product line was acquired by Solvay Advanced Polymers from BP Amoco in November 2001.MatWeb has an entry for this material dry as molded.
Physical Properties Metric English Comments
Density 1.71 g/cc
0.0618 lb/in³
Dry As Molded
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 169 MPa
24500 psi
ASTM D638
Tensile Modulus 13.8 GPa
2000 ksi
ASTM D638
Flexural Yield Strength 230 MPa
33400 psi
ASTM D790
Flexural Modulus 13.1 GPa
1900 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Melt Temperature 321 - 338 °C
610 - 640 °F
Injection