Solvay Specialty Polymers Algoflon® L101-1 Polytetrafluoroethylene (PTFE)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Solvay Specialty Polymers
Trade Name Algoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Algoflon® L101-1 Polytetrafluoroethylene (PTFE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Algoflon® L101-1 is a white PTFE micropowder comprising loose agglomerates of sub-micron sized particles. It exhibits excellent chemical and heat resistance, low surface energy and low coefficient of friction. Algoflon® L101-1 is specially designed for use as an additive in high quality oils and greases. Having higher specific surface area than Algoflon® L203, it can be used in lower concentrations to reduce coefficient of friction and enhance tribological performance of lubricants. Algoflon® L101-1 can be used in inks for improving abrasion, scratch and rub resistance. Additionally it can impart non-stick properties and improve wear-resistance in thermoplastics and coatings.Features: Good Chemical Resistance; High Heat Resistance; Low Friction; Low Molecular WeightUses: Additive; BlendingAdditional Properties: Average Particle Size - Internal Method 3.5 µm; Average Particle Size - Internal Method 0.14 µm; Specific Surface Area - Internal Method > 14 m²/gInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Apparent Bulk Density 0.300 g/cc
0.0108 lb/in³
ASTM D1895
Thermal Properties Metric English Comments
Melting Point 328 - 332 °C
622 - 630 °F
ASTM D3418
Compliance Properties Metric English Comments
FDA Yes
Yes
Descriptive Properties Value Comments
Agency Ratings FDA 21 CFR 177.1550
Availability Asia Pacific
Europe
North America
Color White
Form Powder