Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate

Category Fluid
Manufacturer Solvay
Trade Name SIPOMER®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay SIPOMER® PAM-300 Phosphate Esters of Ppg Monoacrylate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Sipomer PAM-200 incorporated into acrylic resin systems improves adhesion to metallic substrates and glass. Due to its versatile compatibility characteristics with various common solvents and low DAP/MAP ratio, Sipomer PAM-200 can be readily incorporated into various resins including water based, solvent based, and 100% active systems. This monomer has been used mainly in Specialty Purpose Coatings, including industrial maintenance, OEM coil, light industrial, as well as high performance structural adhesives. Sipomer PAM-200 (neutralized version) can also be served as a polymerizable surfactant.Chemical Name: PHOSPHATE ESTERS OF PPG MONOACRYLATEAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: SIPOMER© PAM-300 is an acrylic functional monomer. SIPOMER© PAM-300 can readily copolymerize with various common monomers by radical polymerization to form water-based, solvent-based, or 100% solid resins. Polymers containing this monomer exhibit excellent adhesion properties to various metals and glasses. SIPOMER© PAM-300 has also shown versatile compatibility with a variety of different organic systems. The acrylic functionality of this monomer provides a higher reactivity in radiation cure applications.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
pH 1.5 - 2.0
1.5 - 2.0
1% Solution
Viscosity 8000 - 12000 cP
8000 - 12000 cP
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -40.0 °C
-40.0 °F
Chemical Properties Metric English Comments
Total Acid Number 110 - 115
110 - 115
[mg KOH/g], #1
Processing Properties Metric English Comments
Moisture Content <= 1.0 %
<= 1.0 %
Karl fisher; RP-0327
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Dark Brown, Clean Viscous Liquid
RP-0064
Composition Active Matter
95-97%
MEHQ (Inhibitor)
4500-5500 ppm, RP-1408
Odor Mild Acrylic Odor