Solvay RHODACAL® DS-4 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay RHODACAL® DS-4 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Identification: SODIUM DODECYLBENZENE SULFONATECAS: 69227-09-4 (TSCA) and 11067-82-6 (EINECS/ELINCS)EC Number: 234-289-1Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODACAL DS-4 is a primary anionic emulsifier with a very wide range of applications in emulsion polymerization. RHODACAL DS-4 may be used alone or in combination with other surfactants.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Solids Content 23 %
23 %
pH 7.0 - 8.5
7.0 - 8.5
10% Solution; RP-0420
Surface Tension 32 dynes/cm
32 dynes/cm
at CMC
Optical Properties Metric English Comments
Gardner Color Number <= 5.0
<= 5.0
RP-0138
Chemical Properties Metric English Comments
Ionic Impurities - Fe (Iron) <= 3.0 ppm
<= 3.0 ppm
O-phenanthroline; RP-0277
Processing Properties Metric English Comments
Shelf Life 9.00 Month
9.00 Month
Descriptive Properties Value Comments
Appearance Clear Liquid
RP-0064
Composition Anionic Active
22-23%, MW 348, RP-0033
Formaldehyde
Must Be Negative, RP-0197
Petroleum Ether Extract
<1.0%, RP-0210
Sodium Chloride
<0.25%, RP-0098
Sodium Sulfate
<1.0%, RP-0555
Critical Micelle Concentration 0.001
Foreign Matter Free of Foreign Matter
RP-0636
Ionic Charge Anionic