Solvay GEROPON® HW 15 Surfactant

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name GEROPON®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay GEROPON® HW 15 Surfactant.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description Ethoxylated carboxylates Emulsifier for metal working formulations with excellent dispersing power for calcium soaps. Avoids the formation of insoluble precipitates, and consequently improves the lubricant stability in hard water. Suitable for all water based Metal Working fluids ranging from synthetic and semi-synthetic lubricants to soluble oils.Identification: ALCOHOL ETHO-CARBOXYLATED ACID FORMSolubility Soluble in water. Dispersible in oilsAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: Anionic emulsifier for Metal Working Fluids and lime soap dispersant. GEROPON HW 15 can provide excellent hard water resistance to aqueous Metal working Fluids.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
pH 1.6 - 2.8
1.6 - 2.8
10% aq. Sol.; 540MA3C1E
Thermal Properties Metric English Comments
Flash Point >= 100 °C
>= 212 °F
Optical Properties Metric English Comments
Gardner Color Number <= 6.0
<= 6.0
540MA3C1D
Chemical Properties Metric English Comments
Total Acid Number 69 - 79
69 - 79
[mg KOH/g]; 540MA3C21
Processing Properties Metric English Comments
Moisture Content 6.0 - 10 %
6.0 - 10 %
540MA3C1C
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Yellow liquid to gel
Composition Actives (100-%water-%NaCl)
>89%
NaCl
<1.5%, 540MA3C10
Ionic Charge Anionic