Solvay AMGARD® CT Phosphorus Derivative

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Solvay
Trade Name AMGARD®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay AMGARD® CT Phosphorus Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chemical Name: ORGANIC PHOSPHONATEAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: AMGARD CT is a cyclic phosphonate used to achieve a durable flame retardant finish on polyester fabrics.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Component Elements Properties Metric English Comments
Phosphorous, P >= 19.5 %
>= 19.5 %
RCICP06
Chemical Properties Metric English Comments
Total Acid Number <= 30
<= 30
[mg KOH/g]; RPC90102
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Appearance Clear viscous liquid
Color <150
RPC11004
Composition Dimethyl Methyl PN
<.0999%, RPC90104