Material Notes:
KE-1950-40 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy pumping through most injection molding systems.FeaturesFast cure for increased productivityNo catalyst by-productsCurable over a wide ranger of temperaturesApplicationsO-ringsDiaphragmsCappingRubber rollersConnector packingsOther electrical partsInformation Provided by Shin-Etsu Silicones of America, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
Viscosity 480000 cP
480000 cP
A
480000 cP
480000 cP
B
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
Mechanical Properties Metric English Comments
Hardness, Shore A 42
42
Tensile Strength 9.80 MPa
1420 psi
Elongation at Yield 650 %
650 %
100% Modulus 0.00101 GPa
0.146 ksi
Tear Strength 35.0 kN/m
200 pli
Compression Set 6.0 %

@Temperature 200 °C,
Time 14400 sec
6.0 %

@Temperature 392 °F,
Time 4.00 hour
20 %

@Temperature 150 °C,
Time 3600 sec
20 %

@Temperature 302 °F,
Time 1.00 hour
Processing Properties Metric English Comments
Cure Time 5.00 min

@Temperature 120 °C
0.0833 hour

@Temperature 248 °F
Press Cure
60.0 min

@Temperature 150 °C
1.00 hour

@Temperature 302 °F
Post Cure
Descriptive Properties Value Comments
Appearance Translucent
Cure Rate 44
T10 (302°F, ODR)
63
T90 (302°F, ODR)
Regulatory Testing Class VI, FDA