Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Seals Eastern 5803 Fluoro-silicone

Category Polymer , Thermoset , Fluoropolymer, TS , Thermoset Fluoroelastomer , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Seals Eastern, Inc
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Seals Eastern 5803 Fluoro-silicone.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fluoro-siliconeInformation provided by Seals Eastern, Inc.
Mechanical Properties Metric English Comments
Hardness, Shore A >= 70
>= 70
ASTM D2240, Type A
75
75
AVG; ASTM D2240, Type A
Tensile Strength at Break >= 6.936 MPa
>= 1006 psi
ASTM D412 Method A
7.143 MPa
1036 psi
AVG; ASTM D412 Method A
Tensile Strength, Yield 1.51 MPa
219 psi
AVG Stress at Elongation M25; ASTM D412 Method A
>= 2.36 MPa
>= 343 psi
Stress at Elongation M50; ASTM D412 Method A
2.45 MPa
356 psi
AVG Stress at Elongation M50; ASTM D412 Method A
>= 4.48 MPa
>= 650 psi
Stress at Elongation M100; ASTM D412 Method A
4.57 MPa
663 psi
AVG Stress at Elongation M100; ASTM D412 Method A
Elongation at Break >= 172 %
>= 172 %
ASTM D412 Method A
182 %
182 %
AVG; ASTM D412 Method A
Modulus of Elasticity 0.0112 GPa
1.62 ksi
ASTM D412 Method A
Shear Modulus 0.00372 GPa
0.540 ksi
ASTM D412 Method A
Secant Modulus 0.01016 GPa
1.473 ksi
ASTM D412 Method A
Compression Set 19 %

@Temperature 150 °C,
Time 79200 sec
19 %

@Temperature 302 °F,
Time 22.0 hour
ASTM D395, Test B
Descriptive Properties Value Comments
Strain Energy / Unit Volume at 20% Elongation (psi) 29
Users viewing this material also viewed the following: