Schott Glass 8326 Neutral Glass Tubing

Category Ceramic , Glass
Manufacturer Schott North America
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schott Glass 8326 Neutral Glass Tubing.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Neutral glass tubing, alkali resistance better as for DURAN® Special lab glass The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is less than 100 ppm.Information provided by SCHOTT AG.
Physical Properties Metric English Comments
Density 2.45 g/cc

@Temperature 25.0 °C
0.0885 lb/in³

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Modulus of Elasticity 75.0 GPa
10900 ksi
Poissons Ratio 0.20
0.20
Thermal Properties Metric English Comments
CTE, linear 6.60 µm/m-°C

@Temperature 20.0 - 300 °C
3.67 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Thermal Conductivity 1.20 W/m-K

@Temperature 90.0 °C
8.33 BTU-in/hr-ft²-°F

@Temperature 194 °F
Transformation Temperature, Tg 565 °C
1050 °F
ISO 7884-8
Softening Point 770 °C
1420 °F
Viscosity 10<sup>7.6</sup> dPa s; ISO 7884-3
Working Point 1125 °C
2057 °F
Viscosity 10<sup>4</sup> dPa s; ISO 7884-2
Annealing Point 570 °C
1060 °F
Viscosity 10<sup>13</sup> dPa s; ISO 7884-4
Optical Properties Metric English Comments
Refractive Index 1.506

@Wavelength 587.6 nm
1.506

@Wavelength 587.6 nm
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+6 ohm-cm

@Temperature 350 °C
1.00e+6 ohm-cm

@Temperature 662 °F
2.00e+7 ohm-cm

@Temperature 250 °C
2.00e+7 ohm-cm

@Temperature 482 °F
Dielectric Constant 6.4

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
6.4

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Dielectric Loss Index 0.0065

@Frequency 1.00e+6 Hz,
Temperature 25.0 °C
0.0065

@Frequency 1.00e+6 Hz,
Temperature 77.0 °F
Chemical Properties Metric English Comments
Acid Class, SR 1
1
DIN 12116
Alkali Class, AR 2
2
ISO 695
Descriptive Properties Value Comments
Hydrolytic Resistance Class HGB 1
ISO 719
Stress-optical Coefficient K (10-6mm2N-1) 2.8
DIN 52314
tk100(°C) 210