Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SMAC SMACSONIC® Classic EX Noise and Vibration Damping

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACSONIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACSONIC® Classic EX Noise and Vibration Damping.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
SMACSONIC® is a skin damping range developed to reduce vibrations and induced noise created by a structure. SMACSONIC® is composed of a thin carbon or aluminum plate, SMACTANE® viscoelastic rubber and is a double sided adhesive SMACSONIC® highlights:Skin damping lightweight solutionVery high acoustic insulation performancesWide frequency and temperature rangeDamps flow noise & fuselage flexural modesSMACSONIC® is easy to use and to installThis solution, very effective, light and compact, is easily applicable on structures such as:airplaneshelicoptersvehicleselectronics containersrevolving machinestrainsskisInformation provided by SMAC MontBlac Groupe Technologies
Physical Properties Metric English Comments
Thickness 1900 microns
74.8 mil
Descriptive Properties Value Comments
Constrained layer material Aluminum
Delta 3.2 dB
250 Hz
3.8 dB
1000 Hz
4.2 dB
2000 Hz
4.5 dB
125 Hz
4.6 dB
500 Hz
6.3 dB
4000 HZ
Visoelastic material SMACTANE® EX
Weight 0.61 lbs/sqft