SMAC SMACFOAM® 1250S-02 Damping Material

Category Other Engineering Material
Manufacturer SMAC
Trade Name SMACFOAM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SMAC SMACFOAM® 1250S-02 Damping Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SMAC has developed sound absorbing material dedicated to be used in aerospace and defense activities thanks to its good acoustic properties, its lightweight and its fire resistance properties.Uses: SMAC is able to propose some expertise in the association of foams and solid materials to optimize insulation properties (mass spring mass system). SMACFOAM® can be used to reduce sound transmission and provide sound absorption in tiny, confined but also wide spaces in aircraft, helicopters, battleship, trucks and trains.Features:Lightness and acoustic attenuation propertiesRadiant panel flammability: FAR25-856Max operating temperature: 85°C / 185°FThermal insulationHydrophobic treatment of the foamFoam wih fire resistance properties and compression set performanceSMACFOAM® panels junction can be made with SMACTAPE®MInformation provided by SMAC MontBlac Groupe Technologies
Physical Properties Metric English Comments
Thickness 3160 microns
124 mil
Descriptive Properties Value Comments
Insertion Loss 10 dB
10 dB
14 dB
14 dB
60 dB
61 dB
Overall size 600 x 1000 mm
Weight 0.63 kg/sqm
Copyright © lookpolymers.com All Rights Reserved