Material Notes:
Noryl* SA9000 resin is a modified low molecular weight resin with vinyl end-groups. It is well suited for use with other unsaturated monomers and resins which cure via free radical reactions. These include styrenic, allylic, acrylic, maleimide, methacrylic, and unsaturated polyesters monomers and resins. It has a low solution viscosity and outstanding solubility in toluene & methyl ethyl ketone (MEK). Key application areas are in electronic packaging which include PCB laminates, copper clad laminates, non-epoxy prepregs, and adhesives. The use of Noryl* SA9000 is especially advantageous in insulating materials where very low dielectric properties and decreased moisture absorption are required.
Physical Properties Metric English Comments
Specific Gravity 1.02 g/cc
1.02 g/cc
ASTM D792
Viscosity 160 cP
160 cP
SABIC Method
298 cP
298 cP
SABIC Method
Viscosity Measurement 0.090
0.090
Intrinsic Viscosity [dl/g]; SABIC Method
Thermal Properties Metric English Comments
Transformation Temperature, Tg 160 °C
320 °F
half width; SABIC Method
Electrical Properties Metric English Comments
Dielectric Constant 2.54

@Frequency 1.00e+6 Hz
2.54

@Frequency 1.00e+6 Hz
ASTM D150
Dissipation Factor 0.00070

@Frequency 1.00e+6 Hz
0.00070

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Mn 2300
SABIC Method
Phenolic End-group Content -300ppm
SABIC Method
Physical Form POWDER
SABIC Method
Solubility, Methyl Ethyl Ketone (21°C) 50wt%
SABIC Method
Solubility, Toluene (21°C) 50wt%
SABIC Method
Vinyl Functionality 1.9
SABIC Method